• Amorphous coating was fabricated by using ordinary Co-based self-fluxed alloy powder.
• Amorphous phase accounted for 85.1% of the coating.
• The supercooling liquid region was 44 °C.
An amorphous coating was synthesized on low carbon steel by laser cladding Co-based self-fluxed alloy powder successfully. The microstructure, thermal stability property of the fabricated amorphous coating was investigated. The thickness of amorphous coating was 400 µm while the dendrite zone was only 10 µm height near the interface. The volume fraction of amorphous was 85.1% approximately. DSC curve showed that the glass transition temperature and the crystallization temperature were 298 °C and 342 °C, respectively. The supercooling liquid region was 44 °C which ensured the high thermal stability of amorphous coating against crystallization.
Journal: Materials Letters - Volume 176, 1 August 2016, Pages 306–309