کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
1658794 | 1008361 | 2010 | 6 صفحه PDF | دانلود رایگان |

Refractory metal alloy coatings have been widely used as protective coatings on glass molding dies. The formation of intermetallic compounds in the coatings inhibits grain growth at high-temperature environment in the mass production of optical components. The current work presents Ta–Ru coatings with a Cr interlayer on cemented carbide substrates and silicon wafers deposited by direct current magnetron co-sputtering at 400 °C. The as-deposited Ta–Ru coatings possessed a hardness of 13–14 GPa and a surface roughness of 1.3–4.0 nm. The annealing treatments were carried out at 600 °C under two vacuum levels of 3 × 10− 3 and 3 Pa, respectively. After annealing in vacuum at 3 × 10− 3 Pa, the Ta–Ru coatings showed grain size, hardness, surface roughness and phase stability comparable to those of the as-deposited coatings. While annealing in vacuum at 3 Pa, preferential oxidation of Ta in the Ta–Ru coatings was verified by X-ray photoelectron spectroscopy, a variation of the chemical composition in depth was analyzed by Auger electron spectroscopy and the internal oxidation zone consisting of a laminated structure was observed by transmission electron microscopy.
Journal: Surface and Coatings Technology - Volume 205, Issue 5, 25 November 2010, Pages 1362–1367