کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
1690131 1011251 2008 5 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Diamond deposition on Mo with thermal stress buffer layer coated mild steel substrate by combustion flame CVD
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد سطوح، پوشش‌ها و فیلم‌ها
پیش نمایش صفحه اول مقاله
Diamond deposition on Mo with thermal stress buffer layer coated mild steel substrate by combustion flame CVD
چکیده انگلیسی
In order to develop wear resistance diamond/molybdenum (Mo) hybrid coating process can be conducted in open air. Diamond deposition on the molybdenum with thermal stress buffer layer coated mild steel substrate by the combustion flame chemical vapor deposition (CFCVD) was carried out. As the thermal stress buffer layer, atmospheric plasma sprayed Mo/Fe mixture coating was deposited between Mo top coat and mild steel substrate. Consequently, crack generation and peeling off of the coating occurred due to thermal influences on the condition of Mo coated mild steel substrate in our previous study, diamond particles could be created on the Mo coating without fracture and peeling off. Besides, an additional Mo coating after diamond deposition increases the adhesion force between the diamond coating and the initial Mo coating. This encapsulation of the diamond particles between two Mo layers dramatically improves the resistance of the global coating making it strong enough to resist to the wearing test. These results demonstrate the high potential of thermal sprayed coating for the wear resistance improvement.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Vacuum - Volume 83, Issue 1, 4 September 2008, Pages 102-106
نویسندگان
, , ,