Behaviour of molten beryllium with ITER reference CFC SEPCARB® NB31 under moisture
چکیده انگلیسی

A dramatic exothermic reaction has been observed in Tore Supra with molten aluminium enclosed in a thermally loaded 2D carbon fibre reinforced carbon composite (CFC) tile, exposed after component removal to atmospheric moisture. This led to an important local destruction of the graphite matrix and fibre texture.Beryllium, as aluminium, a carbide forming metal, is foreseen for the ITER first wall armour. Since it can be expected that sputtered, molten and/or evaporated beryllium material will be transported to the hot CFC based divertor surface during normal and off-normal plasma operation, a preliminary reaction experiment has been performed in order to investigate to which extent the Be contaminated graphite matrix and fibre texture of 3D-CFC SEPCARB® NB31 could be locally damaged (“erosion”) following a subsequent long lasting air venting or a supposed in-vessel ingress of coolant (steam) event (ICE).

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Fusion Engineering and Design - Volume 82, Issues 15–24, October 2007, Pages 1688–1693
نویسندگان
, , , ,