A study on the grid-to-rod fretting wear-induced fuel failure observed in the 16×16KOFA fuel
موضوعات مرتبط
مهندسی و علوم پایه مهندسی انرژی مهندسی انرژی و فناوری های برق
پیش نمایش صفحه اول مقاله
A study on the grid-to-rod fretting wear-induced fuel failure observed in the 16×16KOFA fuel
چکیده انگلیسی

The burnup-dependent grid-to-rod gap combined with the fluid-induced vibration may generate grid-to-rod fretting wear-induced fuel failure for some fuel assemblies in a certain burnup range. The systematic grid-to-rod fretting wear-induced fuel failure occurred at the 16×16 Korean Optimized Fuel Assembly loaded in the 2-loop Westinghouse type plant in Korea. Prior to various tests and some measurements for investigating its root causes, they were assumed to be self-excited fuel assembly vibration caused by hydraulic-unbalanced mixing vane design, excessive cross-flow between fuel assemblies during the transition core, or relatively large grid-to-rod gap formation during in-reactor irradiation that may be caused by excessive initial spring force loss of fresh fuel during a fuel rod loading process and/or a fuel assembly transport to a plant and by excessive cladding creep-down. A wide spectrum of tests and some measurements were performed to find out root cause(s) of the grid-to-rod fretting wear-induced fuel failure. Based on these tests and measurements, it is concluded that the self-excited fuel assembly vibration is the primary root cause, while excessive initial spring force loss during the fuel rod loading process is the second major root cause.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Nuclear Engineering and Design - Volume 240, Issue 4, April 2010, Pages 756–762
نویسندگان
,