The heavy metal in the waste can react with sulfur and be converted to metal sulfide through the hydrothermal sulfidation. For metal recovery, the synthetic metal sulfide can be enriched through subsequent flotation process. It is a novel way for the recovery of heavy metal from the sludge. In this study, the effects of liquid/solid ratio, mineralizer concentration, precursor concentration and dosage of sulfur on the sulfidation extent and floatation index were investigated. Result shows that with a precursor concentration of 15%, a Zn/S molar ratio of 1:1.2, a liquid/solid ratio of 3:1, the sulfidation extent of zinc in the sludge was greater than 92%, while the flotation recovery of zinc reached up to 45.34%. The toxicity characteristic leaching procedure (TCLP) revealed that stabilization and detoxification of heavy metals occurred during sulfidation.
Journal: Procedia Environmental Sciences - Volume 16, 2012, Pages 401-408