کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
5370077 | 1388470 | 2006 | 5 صفحه PDF | دانلود رایگان |

Cluster assembled selenium oxide (SeO2) thin films, as a function of oxygen flow pressure (OFP) have been synthesized by a low energy cluster beam deposition (LECBD) technique. The OFP dependent surface morphology leading to well separated nanoclusters (size ranging from 50 to 200 nm) and fractal features are confirmed from transmission electron microscopic (TEM) measurements. A diffusion limited aggregation (DLA) mediated fractal growth with dimension as 1.71 ± 0.01 has been observed for high OFP (60 mbar). Structural analysis by glancing angle X-ray diffraction (GXRD) and selected area diffraction (SAD) studies identify the presence of tetragonal phase SeO2 in the deposit. Micro-Raman studies indicate the shifts in bending and stretching vibrational phonon modes in cluster assembled SeO2 as compared to their bulk counter part due to the phonon confinement effect.
Journal: Applied Surface Science - Volume 253, Issue 4, 15 December 2006, Pages 2138-2142