Fabrication of 2D C/C-SiC composites using PIP based hybrid process and investigation of mechanical properties degradation under cyclic heating
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی مواد
سرامیک و کامپوزیت
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
2D C/C-SiC composites were fabricated using PIP process by repeated impregnations of porous C/C composite preforms with polycarbosilane followed by pyrolysis. Effect of cyclic heating on flexural and shear strength of these composites was studied by exposing the test specimens to oxyacetylene flame for 20Â s and cooling by a blast of air. The cyclic heating tests were repeated up to five times. Average flexural and shear strength of the as fabricated composites were about 330Â MPa and 14.5Â MPa respectively. After five heating and cooling cycles, average flexural and shear strength were reduced to 120Â MPa and 5.5Â MPa respectively. SEM, XRD, EDAX and XPS studies were also carried out to investigate the causes of strength reduction. Oxidation started preferentially at carbon matrix through the cut ends of the weft fibers. Oxidative damage due to repeatedly heating cooling was found to be much smaller in through-thickness direction due to passive oxidation of SiC matrix while severe damage was observed parallel to the fabric layers.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Ceramics International - Volume 43, Issue 3, 15 February 2017, Pages 3414-3423
Journal: Ceramics International - Volume 43, Issue 3, 15 February 2017, Pages 3414-3423
نویسندگان
Suresh Kumar, Bablu M., Ashok Ranjan, L.M. Manocha, N. Eswara Prasad,