کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
615794 881461 2010 7 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Cavitation erosion in silicon nitride: Experimental investigations on the mechanism of material degradation
موضوعات مرتبط
مهندسی و علوم پایه مهندسی شیمی شیمی کلوئیدی و سطحی
پیش نمایش صفحه اول مقاله
Cavitation erosion in silicon nitride: Experimental investigations on the mechanism of material degradation
چکیده انگلیسی

Test samples from three silicon nitride materials used for potential rolling element bearing applications were experimentally studied at different conditions to understand their mechanisms of cavitation erosion. High and low powered ultrasonic vibratory systems were adapted for this study. Variation in the properties and microstructure of test materials helped to identify the mechanisms of wear and the factors that provide resistance to cavitation. Multiple intergranular and transgranular fractures were noted as the initial stages of erosion. Dislodging of grains from the surface led to the formation of small scale pits, resulting in a rough surface, forming a favourable condition for bubble nucleation, which accelerated the damage, eventually dislodging more grains with noticeable pit proliferation and coalescence. Erosion formed a centre wear scar surrounded by pits due to the variation in fluid film thickness. Detailed surface analysis on eroded samples revealed the influence of microstructure on damage initiation and progression. Erosion rate decelerated and remained at a low level of material removal as wear pits grew deeper, creating a bubble cushioning effect.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Tribology International - Volume 43, Issue 12, December 2010, Pages 2251–2257
نویسندگان
, , , ,