Laser induced photocatalytic degradation of hazardous dye (Safranin-O) using self synthesized nanocrystalline WO3
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی شیمی
بهداشت و امنیت شیمی
پیش نمایش صفحه اول مقاله
![عکس صفحه اول مقاله: Laser induced photocatalytic degradation of hazardous dye (Safranin-O) using self synthesized nanocrystalline WO3 Laser induced photocatalytic degradation of hazardous dye (Safranin-O) using self synthesized nanocrystalline WO3](/preview/png/6972666.png)
چکیده انگلیسی
The photocatalytic degradation of Safranin-O (known as Basic Red 2) in water using locally synthesized nanocrystalline WO3 as a photocatalyst was investigated under UV laser irradiation. The photo-oxidation removal of the dye was monitored by UV-vis spectrophotometer. The blank experiments for either laser irradiated only Safranin-O solution or the suspension containing WO3 and Safranin-O in the dark showed that both laser illumination and the photocatalyst were essential for the removal of Safranin-O. The effect of experimental parameters including laser energy, catalyst loading, solution pH and the initial dye concentration on photocatalytic degradation of Basic Red 2 were also investigated. Results indicate that the rate of reaction is strongly influenced by the adsorption of an azo dye into the surface of the photocatalyst materials and suggests an optimum catalyst loading and dye concentration for the degradation reaction. It was investigated that the adsorption of the dye decreases at higher alkaline pH because both catalyst and substrate are negatively charged, developing repulsive forces between them. Kinetic data obtained reveals that the rate of the reaction obeys the first-order kinetics.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Hazardous Materials - Volume 186, Issues 2â3, 28 February 2011, Pages 1226-1233
Journal: Journal of Hazardous Materials - Volume 186, Issues 2â3, 28 February 2011, Pages 1226-1233
نویسندگان
K. Hayat, M.A. Gondal, M.M. Khaled, Z.H. Yamani, S. Ahmed,