کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
7730042 | 1497930 | 2016 | 7 صفحه PDF | دانلود رایگان |
عنوان انگلیسی مقاله ISI
Capacity improvement by deficit of transition metals in inverse spinel LiNi1/3Co1/3Mn1/3VO4 cathodes
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
موضوعات مرتبط
مهندسی و علوم پایه
شیمی
الکتروشیمی
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
Although inverse spinel materials have attracted attention because of their unusually high voltage characteristics, their rechargeable capacities are generally less than 50 mAh gâ1, as a result of the coexistence of Li and transition metal ions at 16d octahedral sites. This work attempted to improve cathode functioning by optimizing the quantities of Li and transition metal ions residing at the 16d sites of LiNi1/3Co1/3Mn1/3VO4. The rechargeable capacity of the LiNi0.28Co0.28Mn0.26V0.80O4 synthesized in the present study was found to be above 120 mAh gâ1, representing the largest capacity reported to date for an inverse spinel material. The results of in-situ XANES analysis demonstrated that the charge-discharge reactions of LiNi1/3Co1/3Mn1/3VO4 corresponds to the Mn2+/Mn4+ and Co2+/Co3+ redox couples, mainly.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Power Sources - Volume 302, 20 January 2016, Pages 240-246
Journal: Journal of Power Sources - Volume 302, 20 January 2016, Pages 240-246
نویسندگان
Ayuko Kitajou, Jun Yoshida, Shinji Nakanishi, Yasuaki Matsuda, Ryoji Kanno, Toshihiro Okajima, Shigeto Okada,