Preparation and characterization of Si3N4/(W, Ti)C nano-composite ceramic tool materials
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی مواد
دانش مواد (عمومی)
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
Si3N4-based composite ceramic tool materials reinforced with nanoscale Si3N4 and microscale (W, Ti)C were fabricated by hot pressing and sintering technology. The flexural strength, fracture toughness and hardness of the sintered composites were tested and the microstructure and indention cracks were observed. The experimental results showed that the Si3N4/(W, Ti)C nanocomposites containing 18 vol% of nanoscale Si3N4 and 20 vol% of microscale (W, Ti)C, which were sintered under a pressure of 30 MPa at 1700 °C in vacuum condition for 45 min, had the optimum comprehensive mechanical properties. The appropriate addition of microscale (W, Ti)C and nanoscale Si3N4 accelerated the formation of elongated β-Si3N4 grains and contributed to the improvement of mechanical properties. The strengthening and toughening mechanisms for the Si3N4/(W, Ti)C composite ceramic tool materials was a synergistic effect of intergranular and transgranular fracture, crack bridging, deflection and branching.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Materials Science and Engineering: A - Volume 596, 24 February 2014, Pages 255-263
Journal: Materials Science and Engineering: A - Volume 596, 24 February 2014, Pages 255-263
نویسندگان
Xianhua Tian, Jun Zhao, Ningbo Zhu, Ying Dong, Jiabang Zhao,