کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
1290175 973320 2008 7 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Electrochemical oxidation of highly oriented pyrolytic graphite during potential cycling in sulfuric acid solution
موضوعات مرتبط
مهندسی و علوم پایه شیمی الکتروشیمی
پیش نمایش صفحه اول مقاله
Electrochemical oxidation of highly oriented pyrolytic graphite during potential cycling in sulfuric acid solution
چکیده انگلیسی

Oxidation of highly oriented pyrolytic graphite (HOPG) under potential cycling conditions is investigated to understand the stability of graphite used in polymer electrolyte fuel cells (PEFCs) under their dynamic operation conditions. Electrochemical methods, AFM and XPS are applied to examine the surface oxidation of HOPG. The current peaks corresponding to quinone–hydroquinone redox reaction begin to appear on cyclic voltammograms after potential cycling between 0.6 V and 0.8 V vs. SHE (standard hydrogen electrode), indicating that the surface of HOPG is partially oxidized to form surface functional groups containing oxygen, whereas HOPG is relatively stable during potential cycling between 0.4 V and 0.6 V. An increase in potential range to 0.8–1.0 V extends the oxidation and forms pits on the surface of HOPG that is caused by the loss of surface carbon through the oxidation to gaseous products. The high rate of potential cycling accelerates the surface oxidation of HOPG.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Power Sources - Volume 185, Issue 2, 1 December 2008, Pages 740–746
نویسندگان
, , , , , ,