Mn3O4 nanoparticles were prepared by a simple solid state decomposition method. Four manganese benzoic acid complexes were synthesized through semi-solid phase reaction method as precursors for the preparation of Mn3O4 nanoparticles. The calcination temperature of the precursors was determined from thermal gravimetrical analyses (TGA). The resulting nanoparticles were characterized by XRD, SEM, STM and HRTEM. The obtained particle size is in the range 39–90 nm. HRTEM indicated the formation of spherical nanoparticles. The optical absorption measurements for the obtained nanoparticles showed that the fundamental absorption edge obeys Tauc's relation for the allowed direct transition. It was found that, the optical band gap (Eg) increases with the decrease of the particle size of the Mn3O4 nanoparticles.
► Synthesis of manganese oxides nanoparticles by using metal complexes as precursors.
► Characterization of the isolated nanoparticles using XRD, SEM, STM, and HRTEM.
► The optical band gap has been calculated and related to the particle size.
Journal: Materials Chemistry and Physics - Volume 137, Issue 2, 14 December 2012, Pages 637–643