چکیده انگلیسی
Stress corrosion cracking (SCC) near the fusion boundary of a 316NG stainless steel (SS) welded joint in high-temperature water was investigated with emphasis on the relation to the microstructural characteristics. δ-Ferrite islands were distributed on the crack paths (grain boundary in the partially melted zone and cell boundary in the unmixed zone) near the fusion boundary of 316NG SS piping. SCC retardation near the fusion boundary was clearly observed in our experiments. The relative crack growth rate (CGR) at the δ-γ interface was estimated to be 0.043 times lower than that at the γ-γ interface. The cracks remained for a considerable period of time just after they reached the δ-ferrite islands. Even those cracks that passed through an initial set of δ-ferrite islands were retarded when they encountered a subsequent set of δ-ferrite islands. High corrosion resistance due to the presence of large amounts of Cr and the island-shaped morphology of δ-ferrite are dominant factors in SCC retardation.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Nuclear Materials - Volume 424, Issues 1â3, May 2012, Pages 57-61
Journal: Journal of Nuclear Materials - Volume 424, Issues 1â3, May 2012, Pages 57-61
نویسندگان
Hiroshi Abe, Yutaka Watanabe,