کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
1566426 1514225 2012 5 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Threshold concentration for H blistering in defect free W
موضوعات مرتبط
مهندسی و علوم پایه مهندسی انرژی انرژی هسته ای و مهندسی
پیش نمایش صفحه اول مقاله
Threshold concentration for H blistering in defect free W
چکیده انگلیسی

Lattice distortion induced by high concentration of H is believed to be precursor of H blistering in single crystalline W (SCW) during H isotope irradiation. However, the critical H concentration needed to trigger bond-breaking of metal atoms presents a challenge to measure. Using density functional theory, we have calculated the formation energy of a vacancy and a self-interstitial atom (SIA) in supersaturated defect-free SCW with various H concentrations. When the ratio of H:W exceeds 1:2, the formation of both vacancies and self-interstitials becomes exothermic, meaning that spontaneous formation of micro-voids which can accommodate molecular H2 will occur. Molecular H2 is not allowed to form, and it is not needed either at the very initial stage of H blistering in SCW. With supersaturated H, the free volume at the vacancy or SIA is greatly smeared out with severe lattice distortion and more H can be trapped than in the dilute H case.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Nuclear Materials - Volume 421, Issues 1–3, February 2012, Pages 176–180
نویسندگان
, , ,