Sr0.13Na0.37Bi0.50TiO3 thin films were prepared by metalorganic solution deposition, and annealed at temperatures from 550 to 700 °C for 1–15 min. The influence of annealing on the morphology, phase and ferroelectric properties was studied by scanning electron microscopy, X-ray diffraction and ferroelectric analyzer. The doping of Na0.50Bi0.50TiO3 films with Sr results in the existence of two phases, i. e., Na0.5Bi0.5TiO3-like (matrix) phase and BiTiO3-like (second) phase, the relative contents of which depend on the annealing conditions. With the increase of annealing temperature and prolongation of annealing time, the phase content of the BiTiO3-like second phase increases and a phenocryst structure was formed, which leads to the decrease of remnant polarization of Sr0.13Na0.37Bi0.50TiO3 thin films.