کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
1619335 | 1005719 | 2010 | 5 صفحه PDF | دانلود رایگان |

Synthesis of SnO2 powder in order to make varistor properties is technologically important. This study aims at examining the process of making nanosized (98.95 − x)SnO2 + 1CoO + 0.05Nb2O5 + xSm2O3 (mol%) (x = 0.05, 0.10, 0.20, 0.50, 1.00 and 2.00) powders using co-precipitation method. Some nanopowders were studied through XRD, SEM and FTIR analyses. The XRD patterns displayed only a tetragonal rutile structure for different molar ratios of samarium oxide (Sm2O3). The mean crystallite size of the sample doped with 0.05 mol% Sm2O3, calcined at 700 °C for 2 h, was about 10 nm. The SEM micrograph of this sample revealed some nanosized spherical particles with a size range of 45–70 nm. The Sm-rich surface prevented the nanoparticles from growing during the calcination at 700 °C.
Journal: Journal of Alloys and Compounds - Volume 495, Issue 1, 9 April 2010, Pages 121–125