Superplasticity of coarse-grained (TiB + TiC)/Ti-6Al-4V composite
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد فلزات و آلیاژها
پیش نمایش صفحه اول مقاله
Superplasticity of coarse-grained (TiB + TiC)/Ti-6Al-4V composite
چکیده انگلیسی
Superplastic deformation of coarse-grained (TiB + TiC)/Ti-6Al-4V composite was carried out at 840-980 °C and 10−4 to 10−2 s−1 in comparison with that of Ti-6Al-4V alloy. The composite had the same optimum superplastic temperature and strain rate as Ti-6Al-4V alloy did. A maximum elongation 462% of the composite was obtained at 920 °C and 10−3 s−1. Based on the microstructure evaluation and the value of activation energy, superplastic mechanism and accommodation mechanism in superplastic deformation of the composite was discussed.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Alloys and Compounds - Volume 490, Issues 1–2, 4 February 2010, Pages 118-123