کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
1660672 | 1008409 | 2008 | 8 صفحه PDF | دانلود رایگان |

The aim of this work was to study if hydrogen environment embrittlement of DIN 1.4301 austenitic stainless steel can be suppressed by a nitrided surface. DIN 1.4301 was plasma nitrided in a N2/H2 discharge. Nitriding produced 3-layered structure consisting of a γN top layer, an intermediate γ/γC-layer and a diffusion layer. It is assumed that the γC phase was formed due to the decomposition of CO originating from the reactor walls and the subsequent incorporation of C into the material. The γC phase is characterized by distinct XRD peaks and carbon contents between 0.5 and 4 wt.% as well as nitrogen contents between 0.5 and 8 wt.%. Plastic deformation of the plasma nitrided specimen showed cracks and some delamination of the γN layer, whereas the γ/γC-layer behaved in a very ductile manner. Even at a plastic deformation of 35% no cracks or any other damage was visible. A tensile test in gaseous hydrogen showed severe embrittlement of the unnitrided steel and the nitrided steel with a γN layer. No cracks were observed in areas where just the γ/γC-layer was present.
Journal: Surface and Coatings Technology - Volume 202, Issue 9, 1 February 2008, Pages 1688–1695