Corrosion behaviour of Sn-containing oxide layer on AZ91D alloy formed by plasma electrolytic oxidation
چکیده انگلیسی
Corrosion phenomenon of magnesium alloys is one of the limits for using magnesium alloys in automotive and aerospace industries. The aim of this study is the development of Sn-containing protective oxide coating by a simple plasma electrolytic oxidation in KOH/KF/Na3PO4 electrolyte on AZ91D magnesium alloy in galvanostatic mode. The film morphology and composition were analysed by SEM coupled with EDS, XRD and Raman spectroscopy. In the oxide, tin is mainly incorporated as crystallised MgSn(OH)6 compound in the layer. The main properties of Sn-containing oxide coating on AZ91D are both keeping the corrosion rate at open-circuit conditions at an acceptable value, and providing a sufficient passivation plateau to reduce the pitting sensibility. The lather characteristic, revealed by pitting tests, addresses the major drawback of magnesium alloys which often undergo important galvanic coupling in service. Consequently, the addition of low stannate concentration in the electrolyte to form Sn-rich anodic oxide on magnesium alloys represents an interesting way to synthesize protective coatings by PEO in a short time of anodization.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Surface and Coatings Technology - Volume 202, Issue 17, 25 May 2008, Pages 4145-4152
نویسندگان
, , ,