Yttrium-substituted bismuth titanate (Bi3.2Y0.8Ti3O12, BYT) thin films were successfully deposited on Pt(1 1 1)/Ti/SiO2/Si(1 0 0) substrates by spin coating with a sol–gel technology and rapid thermal annealing. The effects of annealing temperature (500–800 °C) on microstructure and electrical properties of thin films were investigated. X-ray diffraction analysis shows that the BYT thin films have a bismuth-layered perovskite structure with preferred (1 1 7) orientation. The intensities of (1 1 7) peaks increases with increasing annealing temperature. With the increase of annealing temperature from 500 to 800 °C, the grain size of BYT thin films increases. The highly (1 1 7)-oriented BYT thin films exhibit a high-remnant polarization (2Pr) of 58 μC/cm2 and a low-coercive field (2Ec) of 116 kV/cm, fatigue free characteristics up to >108 switching cycles. The leakage current density (J) were 4.38×10−8 A/cm2 at 200 kV/cm. These results indicate that the highly (1 1 7)-oriented BYT thin film is useful in nonvolatile ferroelectric random access memory applications.
Journal: Journal of Crystal Growth - Volume 310, Issue 10, 1 May 2008, Pages 2520–2524