The Eu2+and Dy3+ activated Sr3Al2O6 (S3A2O-ED) nanophosphors were synthesized by a new microwave method. The S3A2O-ED sample calcined in microwave oven at around 650 °C for 20 min possesses a cubic Sr3Al2O6 single phase. The sample showed small size (80–100 nm) and spherical shape. The excitation and emission spectra indicated that excitation broad band chiefly sited in visible range and the nanophosphors emitted strong light at 611 nm under around 473 nm excitation. Comparing with conventional method, the microwave synthesis of S3A2O-ED greatly decreased the calcining temperature and time. However, the brightness of S3A2O-ED nanophosphors was reduced. The change of luminescent intensity in S3A2O-ED nanophosphors could be attributed to the effect of surface energy.
Journal: Physica B: Condensed Matter - Volume 404, Issue 21, 15 November 2009, Pages 4286–4289