کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
233554 | 465350 | 2012 | 5 صفحه PDF | دانلود رایگان |
Flotation occurs as a result of bubble–particle attachment. This is controlled by the particle surface properties which are created by surface liberation of valuable minerals and collector adsorption within the chemical environment. This paper examines the contribution of both collector dosage and liberation of valuable minerals to bubble–particle attachment time measurements. In order to evaluate particles of different liberation, the bubble–particle attachment time measurements were conducted with a sized fraction of concentrates and tails obtained by flotation of a copper sulfide ore (Northparkes Mine, Australia) in a mechanically agitated batch flotation cell. Quantitative mineral liberation analysis was performed to analyze all concentrates and tails. The results indicated that for particles with high Cu grade, a small increase of collector dosage resulted in a dramatic reduction of attachment time with no further increase on subsequent addition of collector. However, for particles with moderate Cu grade, the effect of collector addition on attachment time was reduced much less because valuable minerals were mainly moderately and poorly liberated. For particles with low Cu grade, collector addition made no difference. All these results confirmed that there is a highly non-linear correlation between mineral liberation, Cu grade, collector dosage and attachment time.
Figure optionsDownload as PowerPoint slideHighlights
► The attachment time was used to study liberation of minerals and collector dosage.
► The attachment time decreased with the increase of collector dosage.
► The attachment time decreased with the increase of Cu grade.
Journal: Minerals Engineering - Volumes 36–38, October 2012, Pages 309–313