کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
234365 465405 2009 5 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Kinetics of high-sulphur and high-arsenic refractory gold concentrate oxidation by dilute nitric acid under mild conditions
موضوعات مرتبط
مهندسی و علوم پایه مهندسی شیمی مهندسی شیمی (عمومی)
پیش نمایش صفحه اول مقاله
Kinetics of high-sulphur and high-arsenic refractory gold concentrate oxidation by dilute nitric acid under mild conditions
چکیده انگلیسی

On one hand, high-sulphur and high-arsenic refractory gold concentrate (HGC) leads to regional ecological damage. On the other hand, it contains a lot of valuable elements. So utilization of it can bring social and environmental benefits. In this paper, the kinetics of HGC oxidation by dilute nitric acid under mild conditions was investigated. The effects of particle size (50–335 μm), reaction temperature (25–85 °C), initial acid concentration (10–30 wt.%) and stirring speed (400–800 rpm) on the iron extraction rate (Cr) were determined. It is obvious that Cr increases with the rise of initial nitric acid concentration, reaction time and stirring speed, but decreases with the increase of particle size. Oxidation kinetics indicates that the rate of reaction is diffusion controlled. The activation energies were determined to be 10.70 kJ/mol in the 10% HNO3 and 12.25 kJ/mol in the 25% HNO3.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Minerals Engineering - Volume 22, Issue 2, January 2009, Pages 111–115