کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
259062 503627 2012 9 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Effect of plastering on the carbonation of a 35-year-old reinforced concrete building
موضوعات مرتبط
مهندسی و علوم پایه سایر رشته های مهندسی مهندسی عمران و سازه
پیش نمایش صفحه اول مقاله
Effect of plastering on the carbonation of a 35-year-old reinforced concrete building
چکیده انگلیسی

A carbonation examination was conducted of a 35-year-old educational building that was located in a subtropical environment. A very important reduction in carbonation was discovered for the columns and beams of building that was plastered (sand–cement render) and/or putted tile/coating. There was no carbonation of the concrete when the plaster (render) thickness surpassed 50 mm. The surface coatings such as tile with high compact and impermeable material may clearly delay the carbonation of concrete. The measured carbonation depth and coefficient of carbonation rate of the building are 8.34 mm and 1.38 mm/(yrs)1/2, respectively.

▸ A carbonation examination was conducted of a 35-year-old building. ▸ The building was plastered and putted tile/coating reduced carbonation. ▸ If the plaster thickness surpassed 50 mm then the concrete had no carbonation. ▸ The surface coatings with tile may delay the concrete carbonation. ▸ This is occurred that tile is an impermeable material.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Construction and Building Materials - Volume 29, April 2012, Pages 206–214
نویسندگان
, , ,