Thermodegradation of medium-chain-length poly(3-hydroxyalkanoates) produced by Pseudomonas putida from oleic acid
موضوعات مرتبط
مهندسی و علوم پایه شیمی شیمی آلی
پیش نمایش صفحه اول مقاله
Thermodegradation of medium-chain-length poly(3-hydroxyalkanoates) produced by Pseudomonas putida from oleic acid
چکیده انگلیسی
Medium-chain-length poly(3-hydoxyalkanoates) (mcl-PHA), comprising six to fourteen carbon-chain-length monomers, are natural thermoplastic polyesters synthesized by fluorescent pseudomonades. In this study, mcl-PHA was produced by Pseudomonas putida from oleic acid in aerobic shake flask fermentation. Thermal degradation of mcl-PHA was performed at temperatures in the range of 160-180 °C. Thermodynamic parameters of mcl-PHA thermal degradation were determined where degradation activation energy, Ed and pre-exponential factor, A equal to 85.3 kJ mol−1 and 6.07 × 105 s−1, respectively; and exhibited a negative activation entropy (∆S) of −139.4 J K−1 mol−1. Titration was carried out to determine the carboxylic terminal concentration and used to correlate number-average molecular weight (Mn) of the polymers. Thermally-degraded PHA contained higher amount of carboxylic terminals and lower Mn compared to the initial PHA and these results coincide with the decreased Mn in GPC analysis. Thermal properties of initial and degraded mcl-PHA were characterized by thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC). The thermal decomposition mechanism was investigated following the analyses of the degradation products using 400-MHz 1H NMR, FTIR spectroscopy and GC analysis. The overall decomposition reaction is the hydrolysis of ester linkages to produce hydroxyl and carboxylic terminals. A small proportion of unsaturated side chain fragments would undergo oxidative cleavage at CC linkages, producing minor amount of low-molecular weight esters and acids. At higher temperatures, the hydroxyl terminal can undergo dehydration to form an alkenyl terminal.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Polymer Degradation and Stability - Volume 95, Issue 12, December 2010, Pages 2334-2342
نویسندگان
, , , ,