The commercial acrylic polymers, Paraloid B72 and Paraloid B67, and a silicon-based product, Dri-Film 104, commonly used as water repellents/consolidants in the restoration of stone artefacts, have been tested to evaluate their performances when submitted to ageing, simulating the outdoor conditions of treated stone. After full characterization, the three polymers were applied as thin films on slides, as thick film on petri dishes and on marble by brush or by imbibition and the resulting samples were submitted to photo-oxidative weathering (λ = 340 nm). The weathering evolution was checked by ultrasonic and colorimetric measurements and by FT-IR, NMR and SEC determinations. Removability tests were also performed. All the polymers underwent irreversible modifications with reduction of their conservative properties, colour change and, above all, impossibility of their complete removal.
Journal: Polymer Degradation and Stability - Volume 91, Issue 12, December 2006, Pages 3083-3096