The use of polymeric blends can increase the range of structures and properties of selective laser sintering (SLS) parts. This study investigates the processing of a binary polar system using polyamide 6 (PA6) and polyamide 12 (PA12) by SLS. The mixture composition and processing conditions, and their influence on the dynamic mechanical properties of the specimens manufactured were evaluated. The maximum tan δ values suggest that PA6 and PA12 have similar visco-dissipative behavior. The PA6/PA12 blends behavior varied according to the relaxation phenomena of the pure components, proportionally to the blend composition. The creep test showed that blends with a higher amount of PA6 had greater plastic deformation and less elastic recovery. In the fatigue test the 20/80 and 50/50 blends presented good fatigue resistance under the test conditions.
Journal: Polymer Testing - Volume 31, Issue 3, May 2012, Pages 411-416