عنوان انگلیسی مقاله ISI
Effect of small amount of poly(ethylene naphthalate) on isothermal crystallization and spherulitic morphology of poly(trimethylene terephthalate)
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه
شیمی
شیمی آلی
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
The effect of a small amount of poly(ethylene naphthalate) (PEN) in its blends with poly(trimethylene terephthalate) (PTT) on isothermal melt-crystallization kinetics and spherulitic morphology of the blends was thoroughly investigated. The maximum PEN content in the blends was 9 wt%. Due to the single composition-dependent glass transition temperature (Tg) that was observed for each blend, these blends appeared to be miscible in the amorphous state. After isothermal crystallization from the melt state, the neat PTT and its blends with PEN exhibited either double or triple melting endotherms. The triple endothermic peaks were observed in both the neat PTT and the blends when being crystallized at crystallization temperatures (Tc) of less than or equal to â¼195 °C. The equilibrium melting temperature (Tm0) for the neat PTT was determined based on the linear Hoffman-Weeks extrapolative method to be â¼248 °C. Such values for the blends were found to decrease with the addition and increasing amount of PEN. Both the neat PTT and the blends were isothermally crystallized over the Tc range of 190-205 °C. At a given Tc, the 97PTT/3PEN blend exhibited a half-time of crystallization (t0.5) value that was lower, while it exhibited reciprocal half-time (t0.5-1), Avrami rate constant (KA), and spherulitic growth rate (G) values that were greater, than those of the neat PTT. With further increase in the PEN content, the t0.5 value increased, while the t0.5-1, KA, and G values decreased. Analysis of the G values based on the Lauritzen-Hoffman's (LH) secondary nucleation theory showed that the neat PTT and the 91PTT/9PEN blend exhibited a regime IIâIII transition at â¼194 °C (â¼467.2 K), while no regime transition was observed for the other two blends. The lateral and the fold surface free energies (Ï and Ïe) and the work of chain folding (q) for the neat PTT and the blends were 19.4, 30.2-46.3 erg cmâ2, and 2.4-3.6 kcal molâ1, respectively. Lastly, the effect of both the Tc and the PEN content on morphology and texture of the PTT spherulites was also investigated and the results showed that the texture of the spherulites became coarser with increasing Tc and PEN content.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Polymer Testing - Volume 26, Issue 8, December 2007, Pages 985-1000
Journal: Polymer Testing - Volume 26, Issue 8, December 2007, Pages 985-1000
نویسندگان
Pitt Supaphol, Nattapol Apiwanthanakorn, Pongpipat Krutphun,