کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
584851 877899 2007 16 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Release of Zn, Ni, Cu, SO42− and CrO42− as a function of pH from cement-based stabilized/solidified refinery oily sludge and ash from incineration of oily sludge
موضوعات مرتبط
مهندسی و علوم پایه مهندسی شیمی بهداشت و امنیت شیمی
پیش نمایش صفحه اول مقاله
Release of Zn, Ni, Cu, SO42− and CrO42− as a function of pH from cement-based stabilized/solidified refinery oily sludge and ash from incineration of oily sludge
چکیده انگلیسی
A framework for the evaluation of leaching behavior of inorganic constituents from stabilized/solidified refinery oily sludge and ash produced from incineration of oily sludge with cement was employed. Metal and anion release as a function of pH was investigated. The leaching test consisted of multiple parallel extractions at pH range from 2 to 12. Remarkably good immobilization >98% was observed for metals of solidified ash at pH > 6 and >93% of solidified oily sludge at pH > 7. Sulfate leaching was high at pH range 2-12. The leaching behavior of metals and anions was simulated by VMINTEQ. The calculations showed that leaching behavior of Zn, Ni and Cu was controlled by chemical equilibrium and surface complexation onto ferrihydrite, at the pH range 2-12. The dominant solid phases that controlled metal leachability were metal hydroxides. The dominant mechanism that described sulfate leaching was found to be chemical equilibrium. Sulfate and also chromate leachability was controlled by Ettringite and Cr(VI)Ettringite as the major minerals affecting their release.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Hazardous Materials - Volume 141, Issue 3, 22 March 2007, Pages 591-606
نویسندگان
, ,