In vitro degradation behavior of M1A magnesium alloy in protein-containing simulated body fluid
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی مواد
بیومتریال
پیش نمایش صفحه اول مقاله
چکیده انگلیسی
Magnesium alloys possess unique advantages to be used as biodegradable implants for clinical applications. In this study, in vitro cells responses and degradation behaviors of magnesium alloy M1A in simulated body fluid (SBF) and albumin-containing SBF (A-SBF) were systematically investigated. Cell responses, in terms of Cell morphology and cell proliferation, imply that M1A possesses good viability for MG63 cells. The corrosion behaviors of M1A are strongly affected by the addition of albumin through the combined effects of adsorption and chelation. Electrochemical testing indicates that such an absorbed albumin layer makes M1A to be more noble with a smaller corrosion current. Corrosion rate monitored by hydrogen evolution rate suggests that the quickly adsorbed albumin serves as an effective protective layer, resulting in a much slower hydrogen release rate at initial stage. With increasing immersion time, a higher corrosion rate is observed since the chelation effect exerts more significant acceleration effects on the removal of the passivation layer. The corrosion mode evaluated by surface morphology of the samples changes from a nonuniform-anisotropic mode for M1A in SBF to a uniform-isotropic mode for M1A in A-SBF.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Materials Science and Engineering: C - Volume 31, Issue 3, 8 April 2011, Pages 579-587
Journal: Materials Science and Engineering: C - Volume 31, Issue 3, 8 April 2011, Pages 579-587
نویسندگان
Yongsheng Wang, Chu Sing Lim, Chao Voon Lim, Ming Shyan Yong, Eng Kiong Teo, Law Ngai Moh,