Catalytic and thermal oxidative pyrolysis of LDPE in a continuous reactor system
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
موضوعات مرتبط
مهندسی و علوم پایه
شیمی
شیمی آنالیزی یا شیمی تجزیه
پیش نمایش صفحه اول مقاله

چکیده انگلیسی
In this work, low-density polyethylene (LDPE) plastic which is a mager product within plastics and formed a high amount of waste was chosen as a material to be worked. LDPE was both decomposed thermally and catalytic in a continuous reactor via as an oxidative media. Catalytic and thermal processes were investigated at the temperature range of 400-500 °C and raw material feeding at a rate of 0.7 g minâ1. As a result of degradation, the maximum liquid yield, acid and peroxid numbers of liquid products in thermal and catalytic oxidative media at 400 °C temperature and 600 mL minâ1 air flow rate conditions have determined as 102%, 28, 52 and 75%, 16 and 43, respectively. In addition, the molecular weight of liquid products were determined by GC/MS system and found that oxygenic compounds for thermal and catalytic oxidative pyrolysis aproximately 50 and 27%, respectively.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Analytical and Applied Pyrolysis - Volume 78, Issue 1, January 2007, Pages 7-13
Journal: Journal of Analytical and Applied Pyrolysis - Volume 78, Issue 1, January 2007, Pages 7-13
نویسندگان
Adil Koç, Ali Y. Bilgesü,