Seal glass compatibility with bare and (Mn,Co)3O4 coated AISI 441 alloy in solid oxide fuel/electrolyzer cell atmospheres
موضوعات مرتبط
مهندسی و علوم پایه شیمی الکتروشیمی
پیش نمایش صفحه اول مقاله
Seal glass compatibility with bare and (Mn,Co)3O4 coated AISI 441 alloy in solid oxide fuel/electrolyzer cell atmospheres
چکیده انگلیسی

To understand seal glass compatibility with interconnect materials in solid oxide fuel/electrolyzer cell environments, a SrO–La2O3–Al2O3–SiO2 (SABS-0) seal glass is bonded with bare AISI 441 alloy and (Mn,Co)3O4 coated AISI 441 alloy; the bonded samples are thermally treated in air and H2/H2O atmospheres at 800 °C for 1000 h. Alloy oxidation, diffusion of the AISI 441/SABS-0 sample elements, chemical reaction, (Mn,Co)3O4 coating stability, and SABS-0 glass devitrification contribute to the interfacial interaction. The interfacial compatibility with the bare AISI 441 alloy is better than with the (Mn,Co)3O4 coated AISI 441 alloy. The thermal treatment atmospheres have no significant effect on the interfacial stability for the bare AISI 441alloy. For the (Mn,Co)3O4 coated AISI 441 alloy, the interfacial stability is better in the H2/H2O atmosphere.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: International Journal of Hydrogen Energy - Volume 35, Issue 21, November 2010, Pages 11908–11917
نویسندگان
, ,