کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
1332308 | 979037 | 2008 | 7 صفحه PDF | دانلود رایگان |

Two alternative methods to prepare organically modified porous hydroxyapatites following a “one pot” approach were compared. The partial substitution of inorganic phosphates by alkylphosphonates leads to mesoporous materials with high specific surface area (>200 m2 g−1). The incorporation of the organic moieties within the hydroxyapatite structure is confirmed by Infra-red and solid-state NMR spectroscopy and depends on the nature of the alkyl chain. However, it induces a significant loss of the material crystallinity. In contrast, the introduction of citrate, a calcium-chelating agent, to the precursor solution does not improve the material specific surface area but allows a better control of the hydroxyapatite structure, both in terms of crystallinity and pore size distribution.
Evolution of pore size distribution of hydroxyapatite (HAp) after alkylphosphonate grafting (20% TPOH) or citrate addition (c-HAp) demonstrates the formation of organically modified mesoporous materials.Figure optionsDownload as PowerPoint slide
Journal: Journal of Solid State Chemistry - Volume 181, Issue 4, April 2008, Pages 848–854