A series of novel water-soluble hemicellulosic derivatives, containing carbamoylethyl and carboxyethyl groups, were heterogeneously synthesized from wheat-straw hemicelluloses with acrylamide (AA) under alkaline conditions. The factors such as reaction temperature, reaction time, molar ratio of catalysis to xylose unit in hemicelluloses and molar ratio of acrylamide to xylose unit in hemicelluloses, were investigated. The average degree of substitution (DS) was calculated by 1H NMR spectroscopy. DS values up to 0.23 in a one-step synthesis of hemicelluloses derivatives were obtained. Under optimum conditions (60 °C, NaOH to xylose unit in hemicelluloses molar ratio of 0.8, AA to xylose unit in hemicelluloses molar ratio of 8.0, reaction time of 1 h) an expected ratio of carbamoylethyl group to carboxyethyl group of 4.8 in the hemicellulosic derivatives was obtained. The structural features of the hemicellulosic derivatives were characterized by FTIR, NMR spectroscopy, and by elemental analysis. The current work provides a facile method for the synthesis of hemicellulose derivatives with bifunctional groups, which could be used as wet-end additives in the papermaking industry.
Figure optionsDownload as PowerPoint slide
Journal: Carbohydrate Research - Volume 343, Issue 16, 3 November 2008, Pages 2776–2782