کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
1398412 | 984377 | 2009 | 7 صفحه PDF | دانلود رایگان |
A one-pot synthetic method to produce aromatic polyimides with high molecular weights from corresponding diamines and dianhydrides was developed, in which polyphosphoric acid (PPA) played a role of an excellent media for one-step synthesis of completely cyclized polyimides. The polymerization was carried out in the solid content of 10 wt/v% at 220 °C. The resulting products exhibited a homogeneous solution in the non-volatilizable PPA instead of precipitation form of the polyimides. The content of P2O5 in PPA had an influence on the molecular weight of the products, and the high percentage of P2O5 resulted in the relative high inherent viscosity. FTIR and Carbon-13 NMR were employed to analyze the structures and TGA was used to evaluate the thermal stability. The polyimides prepared by this one-step route exhibited good thermal properties and high values of activation energies for the degradation, on comparison with the polyimides prepared in DAMc by two-step polymerization method.
Figure optionsDownload as PowerPoint slide
Journal: European Polymer Journal - Volume 45, Issue 10, October 2009, Pages 2805–2811