The compound CaKCe(PO4)2 was obtained using respectively the ceramic method, the Pechini method and the hydrothermal method. The low-temperature (Pechini and hydrothermal) methods yielded homogenous powders with a crystallite size up to 24 nm.The compound has a hexagonal structure with parameters of an elementary cell: a = b = 7.0468(8) Å and c = 6.4367(0) Å. The CaKCe(PO4)2 phosphate occurs in one polymorphic form.A phase equilibrium diagram of the CaKPO4–CePO4 system has been established on the basis of XRD, DTA/DSC/TGA results. The initial phosphates were found to form one intermediate compound, CaKCe(PO4)2, with molar ratio CaKPO4:CePO4 = 1:1, melting incongruently at a temperature of 1530 °C according to the reaction: CaKCe(PO4)2(cr) → CePO4(cr) + L. At a temperature of 1440 °C an eutectic was found to be present in the CaKPO4–CePO4 system at x(CePO4) = 0.25.
► Thermal behavior of samples in CaKPO4–CePO4 system has been studied.
► The CaKCe(PO4)2 phosphate exists in one structural form and is thermally unstable.
► Nanocrystals of CaKCe(PO4)2 were obtained by Pechini and hydrothermal methods.
► Phase diagram of CaKPO4–CePO4 system has been proposed.
Journal: Journal of Alloys and Compounds - Volume 555, 5 April 2013, Pages 138–144