BackgroundUniaxial biomechanical testing of sutures and devices remains the gold standard as in-vivo testing is currently not feasible. The purpose of this study was thus to biomechanically test non-absorbable Ethibond 2-0.Materials and MethodsIn nine porcine menisci, a bucket-handle tear was created and a repair was performed in a vertical inside-out technique using a 2-0 Ethibond suture. The menisci were clamped to a mechanical testing system and gap formation was recorded using a high-resolution digital camera. Vertical displacement, load-to-failure were measured and stiffness was calculated.ResultsThe initial displacement was 5.89 ± 1.42 mm with increasing displacement between 1 and 500 cycles. The increase between cycle 300 and 500 was 0.22 mm and was lower than between cycle 1 to 300 (p = 0.21) whereas the increase between cycle 100 and 300 was not significantly different from 1 to 100 (p = 0.41). The suture failed at 60.5 ± 7.9 N. The stiffness was 19.4 ± 7.8 N/mm.ConclusionsIn conclusion, the EthibondTM 2-0 vertical repair yields satisfactory biomechanical results compared to other sutures.
Journal: Sport-Orthopädie - Sport-Traumatologie - Sports Orthopaedics and Traumatology - Volume 29, Issue 2, May 2013, Pages 118–121