Utilization of fly ash to improve the quality of the acid mine drainage generated by oxidation of a sulphide-rich mining waste: Column experiments
موضوعات مرتبط
علوم زیستی و بیوفناوری علوم محیط زیست شیمی زیست محیطی
پیش نمایش صفحه اول مقاله
Utilization of fly ash to improve the quality of the acid mine drainage generated by oxidation of a sulphide-rich mining waste: Column experiments
چکیده انگلیسی

The production of Acid Mine Drainage (AMD) as a result of the oxidative dissolution of sulphides is one of the main pollution problems affecting natural watercourses in mining environments with sulphide-rich residues. In this work, the generation of AMD was prevented by means of the addition of fly ash to sulphide-rich residues in non-saturated column experiments. A column experiment filled with a pyrite-rich sludge with artificial irrigation leached acid drainages (pH approx. 2) containing high concentrations of sulphate, iron and other metals. However, non-saturated column experiments filled with pyritic-rich sludge and fly ash drained leachates characterized by alkaline pH (pH up to 10), low sulphate concentration, and lack of iron and other metals in solution. The pyrite oxidative dissolution at high pH, as a consequence of the leaching of fly ash, favours the metal precipitation inside the column (mainly iron), the coating of pyrite grains, and the attenuation of the oxidation process, resulting in a great improvement in the quality of the leachates.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Chemosphere - Volume 67, Issue 8, April 2007, Pages 1637–1646