کد مقاله | کد نشریه | سال انتشار | مقاله انگلیسی | نسخه تمام متن |
---|---|---|---|---|
5202569 | 1381904 | 2012 | 10 صفحه PDF | دانلود رایگان |
عنوان انگلیسی مقاله ISI
The influence of metal hydroxide fire retardants and nanoclay on the thermal decomposition of EVA
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
موضوعات مرتبط
مهندسی و علوم پایه
شیمی
شیمی آلی
پیش نمایش صفحه اول مقاله
چکیده انگلیسی
STA-FTIR spectra were deconvoluted to give profiles of individual species' evolution as a function of temperature, in order to identify the individual processes involved. The first step of the degradation, the loss of acetic acid by chain stripping, has been shown to be accelerated by the presence of clay but changed to a loss of acetone by mineral filler fire retardants. This is ascribed to the catalytic properties of the freshly formed alumina and magnesia surfaces. The products of the second step of decomposition are also changed by the various additives.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Polymer Degradation and Stability - Volume 97, Issue 11, November 2012, Pages 2231-2240
Journal: Polymer Degradation and Stability - Volume 97, Issue 11, November 2012, Pages 2231-2240
نویسندگان
Artur Witkowski, Anna A. Stec, T. Richard Hull,