Investigation of the propensity of sulfide concentrates to spontaneous combustion in storage
موضوعات مرتبط
مهندسی و علوم پایه مهندسی شیمی بهداشت و امنیت شیمی
پیش نمایش صفحه اول مقاله
Investigation of the propensity of sulfide concentrates to spontaneous combustion in storage
چکیده انگلیسی

Spontaneous combustion of sulfide concentrates can cause many serious problems during storage. In this study, two representative samples (sulfur-rich sulfide concentrate and iron-rich sulfide concentrate) were investigated for the self-heating behavior using the crossing-point temperature (CPT) method. The corresponding apparent activation energies were determined, 13.7366 kJ/mol for iron-rich sulfide concentrate and 21.3817 kJ/mol for sulfur-rich sulfide concentrate. Furthermore, the surface temperatures of sulfide concentrate stockpiles in different seasons were also measured by a thermal image apparatus. It was found the temperature for iron-rich sulfide concentrate stockpile was higher than that for rich-sulfur sulfide concentrate stockpile. These research results show iron-rich sulfide concentrate exhibits stronger propensity to spontaneous combustion than sulfur-rich sulfide concentrate. Particular attention should be paid to the fire hazard of iron-rich sulfide concentrate in daily safety check work. The combination of the CPT method with the infrared thermal image measurement provides a new approach for the risk assessment on the propensity of sulfide concentrates to spontaneous combustion during the production, storage and transportation. The useful data and experience achieved in this investigation can be also referenced in similar cases later.

Research highlights
► The combination of the crossing-point temperature (CPT) method with the infrared thermal image measurement provides a new approach for the risk assessment of spontaneous combustion of sulfide concentrates production, storage and transportation.
► The study results show iron-rich sulfide concentrate exhibits stronger spontaneous combustion propensity than that of sulfur-rich sulfide concentrate, so particular attention should be paid to the fire hazard of iron-rich sulfide concentrate during the storage.
► Many useful data and experience achieved in this investigation can be referenced in similar cases later.