Investigation of strength and reduction reactivity during heat treatment in simulated-experimental blast furnace of carbon-containing pellet prepared by vapor deposition of tar to cold-bonded pellet with large particle size
ترجمه فارسی عنوان
بررسی قدرت واکنش پذیری و کاهش واکنش پذیری در طول عملیات حرارتی در کوره انفجار شبیه سازی شده کوره پودر حاوی کربن، تهیه شده توسط پودر بخار تار به پودر سرد با اندازه بزرگ ذرات
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی شیمی
مهندسی شیمی (عمومی)
چکیده انگلیسی
Optimum conditions for preparing carbon-containing pellets with a high crushing strength and high reactivity using three kinds of cold-bonded pellets (CPs) prepared by different methods are investigated in this study. The carbon-containing pellets, which have a size fraction suitable for blast furnace are prepared by completely filling the pores in CPs with carbonaceous materials derived from coke oven gas (COG) tar by the vapor deposition (VD) method. A flow-type quartz fixed-bed reactor is used for this method, using a combination of tar pyrolysis at 700â¯Â°C and VD at 350â¯Â°C. The changing pore size distribution, distribution of the carbonaceous material, and crushing strength of the VD samples are then measured for the prepared composites. The carbonaceous materials derived from COG tar completely fills into the mesopores and macropores of the CPs, which is prepared by using Portland cement (PCB) or Carboxymethyl cellulose (CMC), as the binder, and the aging method in stainless-steel container, with increasing VD treatment time. When PCB is treated by the VD method, the C content and crushing strength tends to increase with increasing VD treatment time, and reached 16â¯wt%-dry and 45â¯daN, respectively, until 60â¯min; these values are comparable to the strength of metallurgical-coke with DI1506â¯=â¯87.1. Additionally, carbonaceous materials are uniformly deposited in the particles inside. The changes in the reduction behavior and crushing strength of the prepared VD sample under various heat conditions (simulation-values in experimental-blast furnaces in COURSE50 project). The reduction extent of the VD samples prepared from PCB reaches up to 30-40% at 850â¯Â°C. These rates increase above 850â¯Â°C and attain a value >95% until 950â¯Â°C irrespective of the heating and atmospheric conditions. Fe2O3 and Fe3O4 in the VD samples are reduced to FeO and/or α-Fe until 850â¯Â°C under any condition used, while FeO is completely reduced to α-Fe by 950â¯Â°C. The cold crushing strength of VD samples is maintained up to 850â¯Â°C. Although this value drastically decreases at 900â¯Â°C, which is the temperature at which α-Fe formation occurred, there is no decrease in strength for the reduction of Fe2O3 to Fe3O4, which has been observed reduction disintegration occurs in a conventional blast furnace.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Fuel Processing Technology - Volume 176, July 2018, Pages 21-32
Journal: Fuel Processing Technology - Volume 176, July 2018, Pages 21-32
نویسندگان
Yuuki Mochizuki, Naoto Tsubouchi, Tomohiro Akiyama,