Titania aerogel prepared by low temperature supercritical drying
موضوعات مرتبط
مهندسی و علوم پایه مهندسی شیمی کاتالیزور
پیش نمایش صفحه اول مقاله
Titania aerogel prepared by low temperature supercritical drying
چکیده انگلیسی

Mesoporous titania aerogel with high surfaces area (1086 m2 g−1) were prepared by two steps: heterogeneous precipitation of aqueous solution containing TiOSO4 and ammonia, followed by continuous supercritical extraction with CO2 after replacement of the water with n-propanol/benzene mixture. The total pore volume of as obtained aerogel is 3.44 cm−3 g−1 and the main pore diameter is 20–80 nm. The structure evolution of titania aerogel during heating was studied by DTA and high temperature XRD analyses. At 450 °C titania aerogel transforms to polycrystalline anatase. The morphology and microstructure characteristics of both titania aerogel and anatase samples were obtained by SEM, HRTEM, BET and BJH methods. Anatase reveals high photocatalytic activity during the degradation of 4-chlorophenol in aqueous suspension.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Microporous and Mesoporous Materials - Volume 91, Issues 1–3, 15 April 2006, Pages 1–6
نویسندگان
, , , ,