The environment-induced cracking of as-cold rolled Ni3(Si,Ti) and Ni3(Si,Ti) with 2Mo in sodium chloride solutions
چکیده انگلیسی
The environment-induced cracking (EIC) of as cold-rolled Ni3(Si,Ti) and Ni3(Si,Ti) with 2Mo has been investigated as functions of applied stress, chloride ion concentration, test temperature, and pH by using a constant load method in NaCl solutions. The EIC susceptibility of both intermetallic compounds increased with increasing Cl− ion concentration and test temperature; and increased with decreasing pH. Both intermetallic compounds had the same transgranular fracture appearance and the relationship between log tf (time to failure) and log lss (steady state elongation rate) became the identical straight line irrespective of applied stress, Cl− ion concentration, test temperature, and pH, which means that lss becomes a relevant parameter for predicting tf. The EIC susceptibility of Ni3(Si,Ti) with 2Mo was lower than that of Ni3(Si,Ti), which showed the beneficial effect of Mo. From the results obtained, EIC of both intermetallic compounds was presumed to take place by hydrogen embrittlement (HE).
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Alloys and Compounds - Volume 639, 5 August 2015, Pages 504-510