ObjectiveThe aim of this study was to assess by using confocal microscopy (CLSM), AFM nano-indentation and microtensile bond strength test (μTBS) the quality of the resin–dentin interfaces created with selected bonding parameters.MethodsDentin conditioned with H3PO4 or EDTA was bonded in ethanol- or water-wet condition using a HEMA-free or HEMA-containing adhesive. The resin-bonded teeth were stored in distilled water (24 h) and sectioned as match-sticks (0.9 mm2) for μTBS. Further resin-bonded teeth were sectioned and analyzed using CLSM, and AFM nano-indentation. The AFM imaging and nano-indentation processes were undertaken using a Berkovich diamond indenter. The modulus of elasticity (Ei) and hardness (Hi) across the interface were evaluated with the specimens in a fully hydrated status. The AFM imaging was performed both in dry and wet conditions for evaluating the shrinkage of the hybrid layer on dehydration.ResultsThe HEMA-containing adhesive applied onto H3PO4-etched ethanol or water-wet dentin created hybrid layers with the lowest biomechanical nano-properties (p < 0.05); no significant differences in μTBS were found between the two wet-bonding techniques (p > 0.05). However, the ethanol-wet bonding reduced the dye penetration into the adhesive layer created with the HEMA-containing adhesive. Hybrid layers with high biomechanical properties, low micropermeability and no shrinkage were only possible when using HEMA-free adhesive applied in ethanol wet-dentin. In particular, a significant increase in Ei and Hi was achieved at the hybrid layer and underneath the resin–dentin interface of ethanol-wet EDTA-treated dentin.SignificanceThe use of HEMA-free adhesives applied onto ethanol-wet dentin may be considered as an alternative and suitable bonding strategy to achieve high quality resin–dentin interfaces.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Dental Materials - Volume 28, Issue 6, June 2012, Pages 622–631
نویسندگان
, , , ,