Panavia F 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures
موضوعات مرتبط
مهندسی و علوم پایه مهندسی مواد بیومتریال
پیش نمایش صفحه اول مقاله
Panavia F 2.0 bonding to contaminated zirconia ceramic after different cleaning procedures
چکیده انگلیسی

ObjectivesThe purpose of this laboratory study was to evaluate the influence of different cleaning methods after saliva contamination and after using a silicone disclosing medium on the resin bond strength to zirconia ceramic. The hypothesis was that the resin-ceramic bond strength and its durability are related to the ceramic surface condition.MethodsPlexiglas tubes filled with composite resin were bonded to air-abraded zirconia ceramic disks using a phosphate monomer containing composite resin. Four surface cleaning methods were used after contaminating the ceramic surface: air abrasion with 50 μm Al2O3 at 2.5 bar pressure for 15 s, cleaning with 37% phosphoric acid for 60 s once or for 30 s twice, or cleaning in 96% isopropanol for 15 s. The specimens of the control group were not cleaned after using the silicone disclosing medium. For each combination 16 specimens were bonded in an alignment apparatus. Subgroups of eight bonded specimens were tested for tensile bond strength (TBS) after storage for either 3 or 150 days combined with 37,500 thermal cycles. The statistical analyses were performed with the Kruskal–Wallis test, followed by multiple pair-wise comparisons using the Wilcoxon rank sum test.ResultsThe mean TBS ranged from 6.6 to 49.9 MPa after 3 days and from 0 to 19.8 MPa after 150 days. Air abrasion of the ceramic surface provided statistically significantly higher bond strengths than the other cleaning methods after 3 and 150 days. Alcohol cleaning of the ceramic did not provide durable bond strengths over time.SignificanceCeramic cleaning methods after try-in procedures have a significant influence on the resin-ceramic bond strength. Air abrasion of contaminated zirconia ceramic is the most effective.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Dental Materials - Volume 23, Issue 4, April 2007, Pages 506–512