کد مقاله کد نشریه سال انتشار مقاله انگلیسی نسخه تمام متن
212612 462057 2012 5 صفحه PDF دانلود رایگان
عنوان انگلیسی مقاله ISI
Characterizing industrially electrowon sticky zinc deposits
موضوعات مرتبط
مهندسی و علوم پایه مهندسی شیمی مهندسی شیمی (عمومی)
پیش نمایش صفحه اول مقاله
Characterizing industrially electrowon sticky zinc deposits
چکیده انگلیسی

Physical, chemical, and microscopic characterization of industrially electrowon zinc was performed with a focus on cataloguing morphological differences between sticky and non-sticky zinc deposits. Preferred crystal deposition plane orientations were analyzed by XRD. The crystal orientations for the sticky samples reveal small angle growth (~ 25°) to the cathode surface. In non-sticky samples, the crystals were oriented at an average of ~ 44° to the cathode surface. Deposit microstructures were studied by SEM and optical microscopy. These revealed flat or basal zinc platelets with a number of pores for the sticky deposits whereas the non-sticky deposits were compact, sharp-edged and featured continuous grains with angular crystal plane depositions. No differences in deposit impurity contents were observed by elemental (ICP) and EDX analyses. Microhardness studies of the deposit cross-sections revealed that the sticky samples were, on average, softer than the non-sticky samples particularly at locations closer to the Al cathode.


► Examination of sticky and non sticky zinc electrodeposits.
► We find that non sticky deposits have more deposit morphology.
► There is a greater variation for initial crystal orientation in non sticky samples.
► Sticky samples are softer.
► There are no apparent differences in impurity content between the two.

ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Hydrometallurgy - Volumes 111–112, January 2012, Pages 136–140
نویسندگان
, , , ,