In-situ and ex-situ degradation of sulfonated polyimide membrane for vanadium redox flow battery application
دانلود مقاله + سفارش ترجمه
دانلود مقاله ISI انگلیسی
رایگان برای ایرانیان
کلمات کلیدی
tetramethylsilaneTMSVRFB1H-NMRPODHydrogen nuclear magnetic resonanceSPES - HOPEsPEEK - speekODA - اتاقIEM - ایامVanadium redox flow battery - باتری جریان ریودکس وانادیمCoulomb efficiency - بازده کولنEnergy efficiency - بهره وری انرژیFourier transform infrared - تبدیل فوریه مادون قرمزtriethylamine - تری اتیلامینDegree of sulfonation - درجه سولفونیتVoltage efficiency - راندمان ولتاژFTIR - طیف سنج مادون قرمزX-ray photoelectron spectroscopy - طیف سنجی فوتوالکتر اشعه ایکسXPS - طیف نگاری فوتوالکترونی اشعه ایکسMembrane - غشاءIon exchange membrane - غشای تبادل یونیSEM - مدل معادلات ساختاری / میکروسکوپ الکترونی روبشیDegradation mechanism - مکانیزم تخریبscanning electron microscope - میکروسکوپ الکترونی اسکنSulfonated polyimide - پلی آمید سولفون شدهSulfonated poly(ether sulfone) - پلی اتیل سولفون سولفون شدهSulfonated poly(ether ether ketone) - پلی کربنات (اتر اتر کتون)TEA - چای
موضوعات مرتبط
مهندسی و علوم پایه
مهندسی شیمی
تصفیه و جداسازی
پیش نمایش صفحه اول مقاله
چکیده انگلیسی
In this work the degradation behavior of sulfonated polyimide-hydrogen type (SPI-H) membrane for vanadium redox flow battery (VRFB) usage was investigated through in-situ and ex-situ measurements. Morphological, mechanical and physico-chemical properties, together with structure information of the SPI-H membrane or its oligomer before and after degradation were characterized. Both optical photographs and SEM images show more serious destruction of surface morphology of SPI-H membrane during in-situ degradation than ex-situ one. Decrease in mechanical property and viscosity average molecular weight of SPI-H membrane after degradation in different immersion solutions verifies that both H+ and V(V) play important roles in accelerating the decomposition. FTIR results demonstrate that -SO3H groups of SPI-H membrane in VRFB aren't destructed. 1H-NMR spectra verify the scission of polymer chain and the hydrolysis of imide ring of SPI-H membrane after degradation. XPS spectra evidence the oxidation of -NH2 groups of one hydrolysis product of SPI-H. According to all the experimental results, the 2-step degradation mechanism including hydrolysis and oxidation of SPI-H membrane in VRFB is proposed.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Journal of Membrane Science - Volume 526, 15 March 2017, Pages 281-292
Journal: Journal of Membrane Science - Volume 526, 15 March 2017, Pages 281-292
نویسندگان
Xiaodong Huang, Yang Pu, Yuqin Zhou, Yaping Zhang, Hongping Zhang,