Crosslinking investigation of polybutadiene thermal degradation by carbon-13 nuclear magnetic resonance
موضوعات مرتبط
مهندسی و علوم پایه شیمی شیمی آلی
پیش نمایش صفحه اول مقاله
Crosslinking investigation of polybutadiene thermal degradation by carbon-13 nuclear magnetic resonance
چکیده انگلیسی
Thermal degradation of polybutadiene (PBD) in anaerobic atmosphere at 250 °C had been studied by carbon-13 nuclear magnetic resonance spectroscopy (13C NMR) before complete crosslinking. In this investigation four types of low molecular weight PBD with different 1,2-vinyl isomer content had been chosen, then pure and mixed samples of PBD were heated in different time periods. 13C NMR spectra showed that two kinds of crosslinking mechanisms occur that both of them produce methyl groups. The first mechanism is a reaction between 1,2-vinyl isomers of two PBD chains, and the second one occurs between 1,2-vinyl isomer of one chain via methylene carbon of cis or trans isomer in another chain. Also 13C NMR results showed that the presence of 1,2-vinyl isomer in the PBD structure is necessary and without it none of the mentioned reactions will occur. Furthermore isomers sequence is another important parameter which affects crosslinking. Results show that cis or trans isomer which is not adjacent to 1,2-vinyl isomer does not take part in crosslinking reaction. Moreover such cis or trans isomer can take part in second mechanism of crosslinking that 1,2-vinyl isomer was attached from head to cis or trans isomer, thus in this arrangement of isomers second mechanism of crosslinking will become dominant rather than first mechanism of crosslinking.
ناشر
Database: Elsevier - ScienceDirect (ساینس دایرکت)
Journal: Polymer Degradation and Stability - Volume 96, Issue 10, October 2011, Pages 1805-1811